Breakthrough Technol Ogies for Solder Pot System
Product Overview:
Product Category:
- Description
- Parameter
-
Use of cast iron solder container with ceramic coating can increase the life span of solder container.
1. New anti-corrosion cast iron solder pot.
● The cast iron wall thickness of 10mm pot resist deformation under heat.
● Cast iron contains large quantities of graphite and it has low humidity so reduces the effect of corrosion. The ceramic coating improves corrosion resistance and surface smoothness, hence; increase the service life of the solder pot.
Devices using new channel and nozzle reduce the amount of oxidation hence effectively cutting operating cost.
1. Lowering oxide slag device.
● Lead-free wave solder oxide slag formation characteristics and improve process measures (Harbin Institute of Technology 2007 Master candidate research topics)
● Inflential factors for oxidafion level:Solder oxidation can be caused by many different factors, some are uncontrollable such as high temperature from soldering. Other factors can be controlled using mechanical measures such as flow rate, drop, cross section, spray of flux etc.
Amount of Oxidation = f(amount of drop, contact area, coefficient of velocity, temperature coefficient)
variable quantity: amount of drop, velocity, contact area
Fixed quantity: soldering temperature:
2. Specific measures to reduce oxidation.
● By controlling the flow rate of the peak, reducing the drop, limiting contact area and shortening the path of movement, we can effectively reduce the oxidation and eliminate the amount of creases produced. We can prevent the generation of black oxide by using dynamic rotation to isolate oxygen.
● Adjust the width of the nozzle according to the width of the PCB hence effectively reducing the solder oxidation
Use of new impeller and passage design increase the smoothness of the peak.
User friendly Software Design
● Good demonstrative chart as interface making it easy to operate;
● Includes trouble shooting information, common problems and solutions in software which helps reduce training cost
● Additional SPC query function result in a more efficient control of the production process and guarantee a more stable performance.
The advantage of mixed preheat
● IR preheating can raise temperature fast and hot air preheating can increase temperature uniformity.
● Mix IR preheating and hot air preheating cannot only raise temp.quickly but also enhance temp. uniformity.
● Mixed preheating goes especially well with water-solulde flux.
Built- in partial selective spraying device● Stepper motor moves in the direction of X and Y axis to achieve partial selective flux spraying through synchronous belt, ball screw and linear guide rail.
● Excellent spray nozzle can realize spot-spray,line-spray and rectangle-spray.
● Cotolled by PC + motion control board,quick respond,high accuracy,programmable and user friendly UI.
● Suitable when spraying area is under 50% of total area,which can save flux by over 50%.
Partial Nitrogen charging device of solder pot
● The partial nitrogen releasing unit can minimal amount of nitrogen to create high concentration of nitrogen around the wave.
● The use of stainless steel nano-porous tube release the nitrogen uniformly and in high concentration.
● The 3 flow meters control the 3 nitrogen tubes with consumption rate at 1 5m3/h and the concentration of nitrogen around the nozzle is about 1000ppm.
● Do not support online detection of nitrogen concentration.
Previous
Next
Previous
Next
CONTACT US
Tel:18915611993
Contact: Deng Xingxing
E-mail:dxx@starsea-sz.com
ADD: Building D, No.26, Yinhuan Road, Changshu National New & Hi-tech Industrial evelopment Zone